Total 3727WZ Polypropylene, Injection Molding Grade
Subcategory: Polypropylene; Thermoplastic
Close Analogs: Total Petrochemicals now includes former Fina and Atofina plastics product lines.
Material Notes: Fina’s new HIGH PERFORMANCE injection molding grade Balanced Properties - Fina 3727WZ strikes an optimum balance between excellent mechanical properties (tensile, flex and impact) and processability making it a superior molding grade for cap and closure applications. Impact Strength - Fina 3727WZ offers improved impact strength. Nucleation - Fina 3727WZ is formulated to provide fast cycle time and improve contact clarity in thin wall multi-cavity molds. Antistat - Fina 3727WZ contains an antistat to help protect molded parts from dust accumulation. FDA - Fina 3727WZ complies with all applicable FDA regulations for food contact applications. Recommended Application - Fina 3727WZ is recommended for large thin wall parts, caps and closures. Processing - Fina 3727WZ resin processes on conventional injection molding equipment with typical melt temperatures of 390-450°F (200-232°C). Data provided by the manufacturer, Total Petrochemicals.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Ultimate
- Elongation at Break
- Modulus of Elasticity
- Flexural Modulus
- Izod Impact, Notched
- Impact Test
- Melting Point
- Vicat Softening Point
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|