Total 3824WZ Polypropylene, Injection Molding Grade
Subcategory: Polypropylene; Thermoplastic
Close Analogs: Total Petrochemicals now includes former Fina and Atofina plastics product lines.
Material Notes: Controlled rheology injection molding homopolymer Nucleation - FINA 3824WZ is engineered with nucleation to provide fast cycle time and improve contact clarity in thin wall multi-cavity molds. Antistat - FINA 3824WZ contains an antistat that will help protect molded parts from dust accumulation. FDA - FINA 3824WZ complies with all applicable FDA regulations for food contact applications. Recommended Applications - FINA 3824WZ is recommended for large thin wall parts, caps, and closures. Processing - FINA 3824WZ resin processes on conventional injection molding equipment with typical melt temperatures of 390-450°F (200-232°C). Data provided by the manufacturer, Total Petrochemicals.
| Available Properties |
- Density
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Ultimate
- Elongation at Break
- Modulus of Elasticity
- Flexural Modulus
- Izod Impact, Notched
- Izod Impact, Unnotched
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|