Total 6234WZ Polypropylene, Injection Molding Grade
Subcategory: Polypropylene; Thermoplastic
Close Analogs: Total Petrochemicals now includes former Fina and Atofina plastics product lines.
Material Notes: Random copolymer blow molding grade Impact Strength -- FINA 6234WZ offers good clarity and impact strength, combined with superior top load strength for hot fill applications. Antistat -- FINA 6234WZ contains antistat to minimize dust accumulation for shelf cleanliness as well as improved mold release. Nucleation -- 6234WZ is nucleated to provide a fast cycle and superior top load strength. High Purity -- FINA 6234WZ features minimum taste and odor, and optimum thermal stability for superior color and processability. FDA -- FINA 6234WZ complies with all applicable FDA regulations and may be used under these provisions for food contact and packaging. Recommended Applications -- FINA 6234WZ is ideal for hot fill, single and multilayer extrusion of blow molded containers for syrups and other food items. Processing -- FINA 6234WZ resin processes on conventional injection molding equipment with typical melt temperatures of 390-450°F (199- 232°C). Data provided by the
| Available Properties |
- Density
- Moisture Vapor Transmission
- Oxygen Transmission
- Melt Flow
- Tensile Strength, Ultimate
- Elongation at Break
- Modulus of Elasticity
- Flexural Modulus
- Izod Impact, Notched
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|