Total 7231M Polypropylene, Blow Molding Grade
Subcategory: Polypropylene; Thermoplastic
Close Analogs: Total Petrochemicals now includes former Fina and Atofina plastics product lines.
Material Notes: Clarified random copolymer blow molding grade Clarified -- FINA 7231M offers the ultimate in clarity and gloss, and superior stiffness. Lubricated -- FINA 7231M offers superior core rod release for ease in processing. High Purity -- FINA 7231M features minimum taste and odor, and optimum thermal stability for superior color and processability. FDA -- FINA 7231M complies with FDA regulation 21 CFR 177.1520 and may be used under the provisions for food contact and packaging. Recommended Application -- FINA 7231M is recommended for blow molded containers for food, drug, cosmetic and toiletry applications requiring exceptional clarity. Processing -- FINA 7231M resin processes on conventional blow molding equipment with typical melt temperatures of 390-450°F (199- 232°C) Data provided by the manufacturer, Total Petrochemicals.
| Available Properties |
- Density
- Moisture Vapor Transmission
- Oxygen Transmission
- Melt Flow
- Tensile Strength, Ultimate
- Elongation at Break
- Modulus of Elasticity
- Flexural Modulus
- Izod Impact, Notched
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|