Total 845 Impact Polystyrene
Subcategory: Polystyrene; Thermoplastic
Close Analogs: Total Petrochemicals now includes former Fina and Atofina plastics product lines.
Material Notes: ATOFINA 845E is a high impact polystyrene designed for the custom sheet market. ATOFINA 845E produces tough, ductile sheet with a rich matte finish. Applications: ATOFINA 845E is material is especially suitable for printing and thermoforming applications. Information provided provided by Total Petrochemicals.
| Available Properties |
- Melt Flow
- Tensile Strength, Yield
- Tensile Modulus
- Falling Dart Impact
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Gloss
|
|
|
|