Total 940E Impact Polystyrene
Subcategory: Polystyrene; Thermoplastic
Close Analogs: Total Petrochemicals now includes former Fina and Atofina plastics product lines.
Material Notes: Description: 940E is a super high impact polystyrene designed for high gloss sheet extrusion and thermoforming applications that require additional toughness. Applications: The combination of high gloss, toughness and high stiffness makes 940E an excellent choice for cups, food packaging, custom sheet and coextrusion applications. Information provided provided by Total Petrochemicals.
| Available Properties |
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Falling Dart Impact
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Gloss
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|