Total Lacqrene® 1250 Crystal Polystyrene
Subcategory: Polystyrene; Thermoplastic
Close Analogs: Total Petrochemicals now includes former Fina and Atofina plastics product lines.
Material Notes: LACQRENE® 1250 is a very high molecular weight crystal polystyrene mainly for the injection molding industry. It is characterized by a very good compromise between molecular weight, heat resistance and fluidity. This results in excellent processing combined with good demolding properties and high mechanical properties. This allows reduced thickness and high processing speed. Application CD boxes, Medical and laboratory items (Petri dishes, test tubes), Cosmetics packaging, LACQRENE® 1250 can also be used in extrusion for various applications. Information provided provided by Total Petrochemicals.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell L
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Charpy Impact Unnotched
- Surface Resistivity per Square
- Dielectric Strength
- CTE, linear 20°C
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|