Total Lacqrene® 2901 Medium Impact Polystyrene
Subcategory: Polystyrene; Thermoplastic
Close Analogs: Total Petrochemicals now includes former Fina and Atofina plastics product lines.
Material Notes: LACQRENE® 2901 is a very easy flowing, medium impact polystyrene for injection molding. The very high flow of this grade allows for the production of thin wall section or long flow path molding on single or multi impression tooling. It is particularly recommended for the production of models. The excellent fluidity and ease of coloring of 2901 finds applications in the production of colored masterbatches giving excellent distributive properties. Application Models, Office equipment - filing trays, Closures, Boxes and lids, Pen bodies, Masterbatches Information provided provided by Total Petrochemicals.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell L
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Izod Impact, Notched (ISO)
- Charpy Impact, Notched
- Surface Resistivity per Square
- Dielectric Strength
- CTE, linear 20°C
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|