Total Lacqrene® 4431 Flame Retardant Polystyrene
Subcategory: Polystyrene; Thermoplastic
Close Analogs: Total Petrochemicals now includes former Fina and Atofina plastics product lines.
Material Notes: LACQRENE ® 4240 is a high impact, flame retardant polystyrene with excellent thermal stability. Application Television back covers Information provided provided by Total Petrochemicals.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Vicat Softening Point
- Processing Temperature
|
|
|
|