Total Lacqrene® 4801
Subcategory: Polystyrene; Thermoplastic
Close Analogs: Total Petrochemicals now includes former Fina and Atofina plastics product lines.
Material Notes: LACQRENE® 4801 is an easy flowing, high impact polystyrene for injection molding. The very good processing characteristics of this grade allows for the production of thin articles with long flow paths or complex shapes. A high level of mechanical properties are retained at very low temperatures (-40°C) which makes this grade particularly suitable for ice cream containers. Applications: Ice cream containers, Models, Presentation boxes, General containers, Medical products Information provided provided by Total Petrochemicals.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Izod Impact, Notched (ISO)
- Charpy Impact, Notched
- Surface Resistivity per Square
- Dielectric Strength
- CTE, linear 20°C
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|