Total Lacqrene® 849 High Impact Polystyrene
Subcategory: Polystyrene; Thermoplastic
Close Analogs: Total Petrochemicals now includes former Fina and Atofina plastics product lines.
Material Notes: LACQRENE®849 is a flame retardant high impact polystyrene, halogen free, fitting the requirements of BS EN 60065:1994. It offers a very high fluidity in combination with very high mechanical properties. Application TV back covers Information provided provided by Total Petrochemicals.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched (ISO)
- Charpy Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|