Total Lacqrene® 852 High Impact Polystyrene
Subcategory: Polystyrene; Thermoplastic
Close Analogs: Total Petrochemicals now includes former Fina and Atofina plastics product lines.
Material Notes: LACQRENE® 852 is a flame retardant, high impact polystyrene, halogen free, with excellent thermal stability. Application Copier, Fax, Printers, Television, decoders, Hi-Fi Information provided provided by Total Petrochemicals.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched (ISO)
- Charpy Impact, Notched
- Vicat Softening Point
- Processing Temperature
|
|
|
|