Total Lacqrene® 856 High Impact Polystyrene
Subcategory: Polystyrene; Thermoplastic
Close Analogs: Total Petrochemicals now includes former Fina and Atofina plastics product lines.
Material Notes: LACQRENE® 856 is a flame retardant high impact polystyrene - halogen free, rated UL 94 V0 @ 3mm. LACQRENE® 856 offers rheological and mechanics properties which permits very large moldings. Application TV audio Internal parts for office equipment, Toner cartridges Information provided provided by Total Petrochemicals.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched (ISO)
- Charpy Impact, Notched
- Vicat Softening Point
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|