Total 4180 Polypropylene, Impact Copolymer
Subcategory: Polypropylene; Thermoplastic
Close Analogs: Total Petrochemicals now includes former Fina and Atofina plastics product lines.
Material Notes: ATOFINA 4180 polypropylene is an impact copolymer with an extra low melt flow. ATOFINA 4180 polypropylene has a very low fluidity providing good melt strength with exceptional impact properties. Application ATOFINA 4180 is designed to be particularly suited for pipe and sheet extrusion, blow molding and corrugated cardboard manufacture. Information provided provided by Total Petrochemicals.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Charpy Impact Unnotched
- Charpy Impact, Unnotched Low Temp
- Izod Impact, Notched
- Izod Impact, Notched, Low Temp
- Deflection Temperature at 0.46 MPa (66 psi)
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|