Total 4280 Polypropylene, Impact Copolymer
Subcategory: Polypropylene; Thermoplastic
Close Analogs: Total Petrochemicals now includes former Fina and Atofina plastics product lines.
Material Notes: ATOFINA 4280 polypropylene is an impact copolymer with a low melt flow. ATOFINA 4280 polypropylene has a low fluidity providing melt strength with excellent impact properties. Application ATOFINA 4280 is designed to be particularly suited for profile and sheet extrusion, extrusion-thermoforming and corrugated cardboard manufacture. Information provided provided by Total Petrochemicals.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Charpy Impact Unnotched
- Charpy Impact, Unnotched Low Temp
- Izod Impact, Notched
- Izod Impact, Notched, Low Temp
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|