Total 4280W Polypropylene, Impact Copolymer
Subcategory: Polypropylene; Thermoplastic
Close Analogs: Total Petrochemicals now includes former Fina and Atofina plastics product lines.
Material Notes: ATOFINA 4280W polypropylene is a nucleated impact copolymer. 4280W has a low fluidity providing melt strength with excellent impact properties. It is nucleated for added stiffness and surface hardness. Application ATOFINA 4280W is designed to be particularly suited for profile and sheet extrusion, extrusion-thermoforming and heavy-duty injection molded applications. Information provided provided by Total Petrochemicals.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Charpy Impact Unnotched
- Charpy Impact, Unnotched Low Temp
- Izod Impact, Notched
- Izod Impact, Notched, Low Temp
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|