Total 4520 Polypropylene, Impact Copolymer
Subcategory: Polypropylene; Thermoplastic
Close Analogs: Total Petrochemicals now includes former Fina and Atofina plastics product lines.
Material Notes: ATOFINA 4520 polypropylene is an impact copolymer. ATOFINA 4520 is characterized by a medium fluidity offering a combination of ease of processing and good manufactured article properties in applications ranging from household to industrial. Application ATOFINA 4520 has been developed for the manufacture of garden furniture, battery cases, and other articles requiring a combination of good stiffness and impact properties. Information provided provided by Total Petrochemicals.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Charpy Impact, Unnotched Low Temp
- Izod Impact, Notched
- Izod Impact, Notched, Low Temp
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|