Total Z9450 Random Copolymer Heat Sealable Grade
Subcategory: Polypropylene; Thermoplastic
Close Analogs: Total Petrochemicals now includes former Fina and Atofina plastics product lines.
Material Notes: ATOFINA Z9470 is a low melting, high ethylene random copolymer with improved color, optics and impact properties. The very low melting point of ATOFINA Z9470 makes it an excellent heat seal layer for oriented films. Z9470 complies with FDA regulations Title 21 CFR Section 177.150 (c) 3.1 and may be used under these provisions for food contact and packaging. Application ATOFINA Z9470 is recommended for use in non-oriented film processes for manufacture of packaging films that require improved optical and impact properties and as a heat seal layer for oriented films. Information provided provided by Total Petrochemicals.
| Available Properties |
- Density
- Moisture Vapor Transmission
- Melt Flow
- Tensile Strength, Ultimate
- Elongation at Break
- 1% Secant Modulus
- Dart Drop
- Heat Seal Strength Initiation Temperarture
- Melting Point
- Haze
- Gloss
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|