Total PPC 9712 Polypropylene, Heterophasic Copolymer
Subcategory: Polypropylene; Thermoplastic
Close Analogs: Total Petrochemicals now includes former Fina and Atofina plastics product lines.
Material Notes: ATOFINA Propylene 9712 is heterophasic copolymer. PPC 9712 is characterized by excellent impact resistance and antistatic properties and has been formulated to allow faster cycling through early demolding.
ATOFINA Propylene PPC 9712 has been developed specifically for the injection molding of crates, pails and other heavy duty applications. Information provided provided by Total Petrochemicals.
| Available Properties |
- Density
- Bulk Density
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Yield
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Izod Impact, Notched (ISO)
- Izod Impact, Notched, Low Temp (ISO)
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Notched
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|