Total PPC 11712 Polypropylene, Heterophasic Copolymer
Subcategory: Polypropylene; Thermoplastic
Close Analogs: Total Petrochemicals now includes former Fina and Atofina plastics product lines.
Material Notes: ATOFINA Propylene 11712 is a nucleated controlled-rheology heterophasic copolymer. PPC 11712 is characterized by good stiffness and impact resistance as well as low shrinkage and low warpage. It has been formulated for excellent antistatic properties.
ATOFINA Propylene PPC 11712 has been developed for high speed injection molding of thin walled packaging containers and household articles. Information provided provided by Total Petrochemicals.
| Available Properties |
- Density
- Bulk Density
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Yield
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Izod Impact, Notched (ISO)
- Izod Impact, Notched, Low Temp (ISO)
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Notched
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|