Total PPR 3022 GT3 Polypropylene, Random Copolymer
Subcategory: Polypropylene; Thermoplastic
Close Analogs: Total Petrochemicals now includes former Fina and Atofina plastics product lines.
Material Notes: ATOFINA Polypropylene PPR 3022 GT3 is a nucleated random copolymer polypropylene with a very high level of clarity and a good impact strength resistance. Application ATOFINA Polypropylene PPR 3022 GT3 is intended for blow molding of containers for food packaging, cosmetics and household goods, extrusion of high clarity sheet. Information provided provided by Total Petrochemicals.
| Available Properties |
- Density
- Bulk Density
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Yield
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Izod Impact, Notched (ISO)
- Charpy Impact, Notched
- Melting Point
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|