Total PPH 3061 Polypropylene, Homopolymer
Subcategory: Polypropylene; Thermoplastic
Close Analogs: Total Petrochemicals now includes former Fina and Atofina plastics product lines.
Material Notes: ATOFINA Polypropylene PPH 3061 is homopolymer polypropylene. Application ATOFINA Polypropylene PPH 3061 is intended for the production of blow molded containers, sheets, high tenacity tapes and twines, tapes for woven sack manufacture and sheet for thermoforming. Information provided provided by Total Petrochemicals.
| Available Properties |
- Density
- Bulk Density
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Yield
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Izod Impact, Notched (ISO)
- Charpy Impact, Notched
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|