Total MR 2002 Polypropylene, Metallocene Polypropylene
Subcategory: Polypropylene; Thermoplastic
Close Analogs: Total Petrochemicals now includes former Fina and Atofina plastics product lines.
Material Notes: ATOFINA Polypropylene MR 2002 is a metallocene polypropylene, and is characterized by high fluidity for high speed spinning on spun laid non-woven lines where spun filaments are produced to form a web that is then thermally bonded to manufacture products for hygienic and technical use. Application ATOFINA Polypropylene MR 2002 has a special ant gas-fading formulation to reduce yellowing in fibers. Information provided provided by Total Petrochemicals.