Total FinaceneTM EOD98-07, Metallocene Isotactic Propylene Polymer
Subcategory: Polypropylene; Thermoplastic
Close Analogs: Total Petrochemicals now includes former Fina and Atofina plastics product lines.
Material Notes: Finacene EOD97-07 is a isotactic form of polypropylene polymer made via ATOFINA proprietary technology . EOD98-07 complies with FDA regulations Title 21 CFR Section 177.1520(c) 1.1b and may be used under these provisions for food contact and packaging. Application Finacene EOD98-07 is recommended for melt spun and spunbond fiber applications. Information provided provided by Total Petrochemicals.
| Available Properties |
- Density
- Melt Flow
- Tenacity
- Elongation at Break
- Melting Point
- Xylene Solubles
|
|
|
|