Finaprene® 1205 Di-block Styrene-Butadiene TPE Copolymer
Subcategory: Elastomer, TPE; Styrene-Butadiene; Thermoplastic
Close Analogs: Total Petrochemicals now includes former Fina and Atofina plastics product lines.
Material Notes: Di-block Styrene-Butadiene Copolymer Description: Finaprene® 1205 is a di-block styrene-butadiene (SB) copolymer. It is perfectly suited to improve adhesion properties of compounds. Applications: Used to improve the general adhesion of the compounds, reduce the blend viscosity, and reduce the dirty marks when cutting labels. Additional Notes: Block Polystyrene: 17.5%; Finaprene 1005 Data provided provided by Total Petrochemicals.
| Available Properties |
- Density
- Mooney Viscosity
- Viscosity Measure
- Styrene Content
- Butadiene Content
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|