Finaprene® 401 Styrene-Butadiene TPE Copolymer
Subcategory: Elastomer, TPE; Styrene-Butadiene; Thermoplastic
Close Analogs: Total Petrochemicals now includes former Fina and Atofina plastics product lines.
Material Notes: Styrene-Butadiene Copolymer Description: Finaprene® 401 is a thermoplastic elastomer type radial styrene-butadiene block copolymer (SBS). It has a moderate molecular weight, thus provides excellent cohesive and elastic properties to the modified road binder. Applications: Thanks to its very high crumb porosity Finaprene® 401 is used for the road binder modification. Its crumb shape, along with the medium molecular weight confer excellent properties along with an easy dispersion and optimum storage stability at high temperature to the modified road binder. Data provided provided by Total Petrochemicals.
| Available Properties |
- Viscosity Measure
- Styrene Content
- Butadiene Content
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|