Finaprene® 507 Styrene-Butadiene TPE Copolymer
Subcategory: Elastomer, TPE; Styrene-Butadiene; Thermoplastic
Close Analogs: Total Petrochemicals now includes former Fina and Atofina plastics product lines.
Material Notes: Styrene-Butadiene Copolymer Description: Finaprene® 507 is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its high styrene content, Finaprene® 507 provides excellent mechanical properties to the compound along with a good fluidity. Applications: Thanks to its high fluidity Finaprene® 507 is designed for the compounding industry. Finaprene® 507 can be used as an alternative to GPPS to provide compounds hardness without imparting other compounds properties such as abrasion resistance or flexural resistance. Data provided provided by Total Petrochemicals.
| Available Properties |
- Density
- Melt Flow
- Styrene Content
- Butadiene Content
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|