Finaprene® 602 Styrene-Butadiene TPE Copolymer Compound

 

Subcategory: Elastomer, TPE; Styrene-Butadiene; Thermoplastic

Close Analogs:

Total Petrochemicals now includes former Fina and Atofina plastics product lines.

Material Notes:
Styrene-Butadiene Copolymer

Description: Finaprene® 602 is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its broad molecular weight distribution, Finaprene® 602 provides good fluidity properties to the compound while keeping good mechanical properties.

Applications: Thanks to it very high crumb porosity Finaprene® 602 is designed for the compounding industry. This crumb shape, along with the broad molecular weight distribution confer a quick oil absorption to the polymer and lead to the production of fluid compounds. This fluidity will enhance the surface aspect of the injected article. The structure of 602 is n = 2, 3, 4, 5.

Content of the compound for which the listed properties apply:
F484: 0
F435: 45
F411x: 25
F602: 30
F507: 0
GPPS: 50
HIPS: 0
Oil: 60
CaCO3: 15

Additional Notes:
DIN Abrasion: 195 mm³

Data provided by Total Petrochemicals.

Available Properties
  • Density
  • Melt Flow
  • Hardness, Shore A
  • Tensile Strength, Ultimate
  • Elongation at Break
  • 300% Modulus
  • Tear Strength
  • Abrasion
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。