Finaprene® 602 Styrene-Butadiene TPE Copolymer Compound
Subcategory: Elastomer, TPE; Styrene-Butadiene; Thermoplastic
Close Analogs: Total Petrochemicals now includes former Fina and Atofina plastics product lines.
Material Notes: Styrene-Butadiene Copolymer Description: Finaprene® 602 is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its broad molecular weight distribution, Finaprene® 602 provides good fluidity properties to the compound while keeping good mechanical properties. Applications: Thanks to it very high crumb porosity Finaprene® 602 is designed for the compounding industry. This crumb shape, along with the broad molecular weight distribution confer a quick oil absorption to the polymer and lead to the production of fluid compounds. This fluidity will enhance the surface aspect of the injected article. The structure of 602 is n = 2, 3, 4, 5. Content of the compound for which the listed properties apply: F484: 0 F435: 45 F411x: 25 F602: 30 F507: 0 GPPS: 50 HIPS: 0 Oil: 60 CaCO3: 15 Additional Notes: DIN Abrasion: 195 mm³ Data provided by Total Petrochemicals.
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- 300% Modulus
- Tear Strength
- Abrasion
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|