Total Finaprene® 411 Thermoplastic Elastomer
Subcategory: Elastomer, TPE; Thermoplastic
Close Analogs: Total Petrochemicals now includes former Fina and Atofina plastics product lines.
Material Notes: Finaprene® 411 is a thermoplastic elastomer type radial styrene-butadiene block copolymer (SBS). Application Thanks to its very high crumb porosity, Finaprene® 411 is designed for the adhesive market. Its high molecular weight confer excellent mechanical properties to the compounds along with optimized rheological properties. Information provided provided by Total Petrochemicals.
| Available Properties |
- Viscosity Measure
- Styrene Content
- Butadiene Content
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|