Total Finaprene® 502 Thermoplastic Elastomer
Subcategory: Elastomer, TPE; Thermoplastic
Close Analogs: Total Petrochemicals now includes former Fina and Atofina plastics product lines.
Material Notes: Finaprene® 502 is a thermoplastic elastomer type linear styrene-butadiene block copolymer (SBS). Thanks to its high styrene content, Finaprene® 502 provides excellent cohesive and elastic properties to the compounds. Application Thanks to its high styrene content Finaprene® 502 is used in the adhesive and compounding application. Its linear structure, along with its high molecular weight confer a performing combination of viscosity, temperature range and mechanical properties. Information provided provided by Total Petrochemicals.
| Available Properties |
- Viscosity Measure
- Styrene Content
- Butadiene Content
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|