Finathene® 3802 HDPE, blow molding, cable
Subcategory: Polyethylene; Thermoplastic; HDPE
Close Analogs: Total Petrochemicals now includes former Fina and Atofina plastics product lines.
Material Notes: FINATHENE® 3802 is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low-pressure slurry polymerization process. FINATHENE® 3802 has been especially developed for the manufacturing of blow molded articles offering a good flexibility. This grade is particularly appropriate for the production of small containers as well as for metallic drum liners. FINATHENE® 3802 is characterized by its excellent resistance to crack formation, low dielectric constant, high hardness and excellent abrasion resistance. FINATHENE® 3802 contains additives to ensure outstanding stability against degradation during processing and long-term product life. FINATHENE® 3802 is best processed at temperatures between 180 and 220°C. Information provided provided by Total Petrochemicals.
| Available Properties |
- Density
- Viscosity
- Environmental Stress Crack Resistance
- Oxidative Induction Time (OIT)
- Melt Flow
- Hardness, Shore D
- Tensile Strength at Break
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break
- Elongation at Yield
- Modulus of Elasticity
- Flexural Modulus
- Tensile Impact Strength
- Volume Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Heat of Fusion
- CTE, linear 20°C
- Specific Heat Capacity
- Melting Point
- Vicat Softening Point
- Brittleness Temperature
- Food Approval
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|