Finathene® 5202 HDPE, blow molding
Subcategory: Polyethylene; Thermoplastic; HDPE
Close Analogs: Total Petrochemicals now includes former Fina and Atofina plastics product lines.
Material Notes: Applications: Bleach and detergents, industrial chemicals, industrial parts, packaging aggressive liquids, food packaging. Blow molding stock temperature 360 - 400°F Extrusion melt temperature 380 - 420°F Information provided provided by Total Petrochemicals.