Finathene® 53080 HDPE, blow molding, sheet
Subcategory: Polyethylene; Thermoplastic; HDPE
Close Analogs: Total Petrochemicals now includes former Fina and Atofina plastics product lines.
Material Notes: Finathene E® 53080 is a high density polyethylene produced by the slurry loop low pressure polymerization process. Finathene E® 53080 has been especially developed for the production of containers to be submitted to the regulations for transportation of dangerous goods. Finathene® 53080 is best processed at temperatures between 180 and 220°C. Information provided provided by Total Petrochemicals.
| Available Properties |
- Density
- Environmental Stress Crack Resistance
- Melt Flow
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Tensile Impact Strength
- Vicat Softening Point
- Food Approval
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|