Finathene® BM 593 HDPE, blow molding
Subcategory: Polyethylene; Thermoplastic; HDPE
Close Analogs: Total Petrochemicals now includes former Fina and Atofina plastics product lines.
Material Notes: FINATHENE® BM 593 is a new generation of bimodal high density polyethylene based on hexene (C6) as co-monomer and is produced by the ATOFINA Double Loop Technology™. FINATHENE® BM 593 has been especially designed for the manufacture of blow molded bottles for aggressive liquids (up to 5 liters). Typical applications are bottles for the packaging of liquid detergents and personal care products. FINATHENE® BM 593 has a broad (bimodal) molecular weight distribution that ensures easy processing, high machine output and bottles with a good surface finish. Due to the combination of hexene (C6) co-monomer and a bimodal molecular weight distribution, FINATHENE® BM 593 offers an excellent balance between stiffness and environmental stress crack resistance. This ensures a high security of stacking during transit and storage of bottles. FINATHENE® BM 593 is best processed at temperatures between 180 and 220°C. Information provided by Total Petrochemicals.
| Available Properties |
- Density
- Environmental Stress Crack Resistance
- Melt Flow
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|