Finathene® WR 201 B N, HDPE, blow molding
Subcategory: Polyethylene; Thermoplastic; HDPE
Close Analogs: Total Petrochemicals now includes former Fina and Atofina plastics product lines.
Material Notes: FINATHENE® WR 201 B N is a high density polyethylene produced by the slurry loop low pressure polymerization process. FINATHENE® WR 201 B N has been developed for the blow molding of Plastic Fuel Tanks and automotive technical parts. FINATHENE® WR 201 B N is suitable for the most common barrier treatments. The material specific characteristics allow to achieve outstanding tank properties, including crash test and fire resistance, with a substantial net weight reduction of the Plastic Fuel Tank. Information provided provided by Total Petrochemicals.
| Available Properties |
- Density
- Environmental Stress Crack Resistance
- Thermal Stress Crack Resistance
- Melt Flow
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Impact Test
- Melting Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|