Lacqtene® 1003 FE 30 HDPE, blow molding
Subcategory: Polyethylene; Thermoplastic; HDPE
Close Analogs: Total Petrochemicals now includes former Fina and Atofina plastics product lines.
Material Notes: Medium density radical polyethylene made by high tubular pressure process for medical applications requiring sterilization : small and medium stiff containers for parental mixtures, ophthalmic solutions, sterilized ampoules. Advised temperature profile : 150 to 180°C Lacqtène 1003FE30 is easily converted on aseptical machines. (Rommelag or similar) Information provided provided by Total Petrochemicals.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength at Break
- Elongation at Break
- Modulus of Elasticity
- Dart Drop Test
- Melting Point
- Vicat Softening Point
- Haze
- Food Status
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|