Lacqtene® FD 0270 LDPE, blown film, compounding, injection molding
Subcategory: Polyethylene; Thermoplastic; LDPE; Polymer
Close Analogs: Total Petrochemicals now includes former Fina and Atofina plastics product lines.
Material Notes: Low density radical polyethylene made by high pressure process. Temperature profile (°C) for injection molding: 200 to 260 Information provided provided by Total Petrochemicals.
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Dart Drop Test
- Melting Point
- Vicat Softening Point
- Haze
- Food Status
|
|
|
|