Finathene® LL 6010 FE 18P LLDPE film
Subcategory: Polyethylene; Thermoplastic; LLDPE; Polymer
Close Analogs: Total Petrochemicals now includes former Fina and Atofina plastics product lines.
Material Notes: Linear low density polyethylene made by gas phase process for blown film applications. Advised temperature profile: 190 to 220°C. Information provided provided by Total Petrochemicals.
| Available Properties |
- Density
- Thickness
- Melt Flow
- Film Tensile Strength at Yield, MD
- Film Tensile Strength at Yield, TD
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Secant Modulus, MD
- Secant Modulus, TD
- Dart Drop Test
- Melting Point
- Haze
- Food Status
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|