Finathene® 3802 Blue HDPE pipe, injection molding
Subcategory: Polyethylene; Thermoplastic; HDPE
Close Analogs: Total Petrochemicals now includes former Fina and Atofina plastics product lines.
Material Notes: FINATHENE® 3802 Blue is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low pressure slurry polymerization process. FINATHENE® 3802 Blue is a blue polyethylene specially developed for the manufacture of pressure pipes and fittings. Its well balanced property profile and composition makes FINATHENE® 3802 Blue perfectly suited for potable water distribution. Information provided provided by Total Petrochemicals.
| Available Properties |
- Density
- Viscosity
- Environmental Stress Crack Resistance
- Oxidative Induction Time (OIT)
- Melt Flow
- Tensile Strength at Break
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break
- Elongation at Yield
- Modulus of Elasticity
- Flexural Modulus
- Charpy Impact, Notched
- Volume Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Heat of Fusion
- CTE, linear 20°C
- Specific Heat Capacity
- Melting Point
- Vicat Softening Point
- Brittleness Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|