Finathene® 3802N Natural HDPE pipe grade
Subcategory: Polyethylene; Thermoplastic; HDPE
Close Analogs: Total Petrochemicals now includes former Fina and Atofina plastics product lines.
Material Notes: Applications: Natural gas distribution, extruded pipes, molded fittings, pipe coating, pipe lining Information provided provided by Total Petrochemicals.
| Available Properties |
- Density
- PENT
- Melt Flow
- Hardness, Shore D
- Tensile Strength @ Break
- Tensile Strength @ Yield
- Elongation at Break
- Flexural Modulus
- Hydrostatic Design Basis @ 73°F
- CTE, linear 20°C
- Melting Point
- Vicat Softening Point
|
|
|
|