Finathene® XSene® XS10 H HDPE, pipe, injection molding
Subcategory: Polyethylene; Thermoplastic; HDPE
Close Analogs: Total Petrochemicals now includes former Fina and Atofina plastics product lines.
Material Notes: FINATHENE® XS 10 H is a high density polyethylene based on C6 hexene as co-monomer and is produced by the Fina Double Loop Technology™. FINATHENE® XS 10 H is a high performance dark blue compound specially developed for potable water distribution. FINATHENE® XS 10 H has a broad bimodal molecular weight distribution that ensures easy processing during extrusion. Due to its high melt strength, FINATHENE® XS 10 H is particularly suited for extrusion of large diameter, thick wall pipes. Information provided provided by Total Petrochemicals.
| Available Properties |
- Density
- Viscosity
- Oxidative Induction Time (OIT)
- Melt Flow
- Tensile Strength at Break
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Specific Heat Capacity
- Melting Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|