Lacqtene® 2006 TN 35 HDPE pipe coating
Subcategory: Polyethylene; Thermoplastic; HDPE
Close Analogs: Total Petrochemicals now includes former Fina and Atofina plastics product lines.
Material Notes: LACQTENE® 2006 TN 35 is a medium density polyethylene produced by the gas phase polymerization process with hexene as comonomer. LACQTENE® 2006 TN 35 may be used for pipe and sheet extrusion (flexible sheets, membranes, liners,...) Information provided provided by Total Petrochemicals.
| Available Properties |
- Density
- Thermal Stress Crack Resistance
- Oxidative Induction Time (OIT)
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched (ISO)
- Melting Point
- Vicat Softening Point
- Food Status
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|