Fine Organics FINALUX G 601 Lubricant Additive
Subcategory: Additive/Filler for Polymer
Material Notes: Applications: Universal internal lubricant for rigid PVC and foamed PVC, applicable independently of stabilizing system. Pseudo-plasticizer for PVC. Low improver and lubricant for PMMAInformation provided by Fine Organics
| Available Properties |
- Additive Loading
- Melting Point
- Influence on Transparency
- Lubricating Effect
- Physical Form
|
|
|
|