Fine Organics FINALUX G 728 Lubricant Additive
Subcategory: Additive/Filler for Polymer
Material Notes: Applications: Internal and external lubricant for PVC cables, films, bottles, lead stabilized injection molded articles. Synergistic co-stabilizing properties with Pb-stabilizers.Information provided by Fine Organics
| Available Properties |
- Additive Loading
- Melting Point
- Influence on Transparency
- Lubricating Effect
- Physical Form
|
|
|
|