Fine Organics FINALUX CL 5 Composite Lubricant
Subcategory: Additive/Filler for Polymer
Material Notes: Applications: Liquid combination lubricant with good compatibility and stronger release properties than FINALUX CL 4 suitable for plasticized PVC extruded and molded articles (high gloss).Information provided by Fine Organics
| Available Properties |
- Additive Loading
- Influence on Transparency
- Lubricating Effect
- Physical Form
|
|
|
|