Firestone CLM200-001 Nylon 6
Subcategory: Nylon; Thermoplastic; Nylon 6
Key Words: PA6; Polyamide 6
Material Notes: Used for monofiliament extrusion. Natural color. Not heat stabilized or modified. Lubricated. Chip size is 2 x 3.5 mm. Information provided by Firestone
| Available Properties |
- Specific Gravity
- Viscosity Measurement
- Linear Mold Shrinkage
- Tensile Strength @ Break
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Moisture Content
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|