TPI PORENE® KU900 Super High Heat ABS
Subcategory: ABS Polymer; Thermoplastic
Material Notes: INJECTION MOLDING. ELECTRICAL PARTS, AUTOMOTIVE APPLICATIONS, HOUSEHOLD GOODS, TOYS Porene® is a registered trademark of Thai Petrochemical Industry Co. LTD. Information provided by Dayson Polymers.