MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

Subscribe to FREE Trade Publications!

Formosa Plastics Formolene HB5502Z Blow Molding HDPE

 

Subcategory: Polyethylene; Thermoplastic; HDPE

Material Notes:
Hexene Copolymer

Applications: Injection blow molded pharmaceutical packaging

Formolene HB5502Z eliminates the need for including a mold release agent at each machine, by incorporating zinc stearate with the resin. This incorporation assures uniform consistent release properties. It may be used as an injection blow molding resin.

Produced using licensor formulation for HHM 5502BZ. Licensor does not warrant or imply that this product meets their specifications for HHM 5502BZ.

Meets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles intended for direct food contact.

Nominal properties reported herein were determined on compression molded specimens prepared in accordance with Procedure C of ASTM D1928. Physical properties are typical of product but do not reflect normal testing variance and therefore should not be used for specification purposes.

Information provided by Formosa Plastics Corporation, USA.

Available Properties
  • Density
  • Environmental Stress Crack Resistance
  • Melt Flow
  • Tensile Strength, Yield
  • Elongation at Break
  • Flexural Modulus
  • Brittleness Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。