Formosa Plastics Formolene L43840U Rotational Molding LLDPE
Subcategory: Polyethylene; Thermoplastic; LLDPE
Material Notes: Butene Copolymer Applications: Toys and other non-tank rotational molding applications. Formolene L43840U is a Butene Copolymer of linear low density polyethylene for toys and other non-tank rotational molding applications. Contains a low level of UV stabilizer. Meets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles intended for direct food contact. Information provided by Formosa Plastics Corporation, USA.
| Available Properties |
- Density
- Environmental Stress Crack Resistance
- Melt Flow
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|